TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Sat, 27 May 2006 07:25:03 -0700
Reply-To:
ZLATKO BIJEDIC <[log in to unmask]>
Subject:
From:
ZLATKO BIJEDIC <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=utf-8
MIME-Version:
1.0
Parts/Attachments:
text/plain (39 lines)
Gold can be "etching resist" for CuCl2/Hcl etching solution, BUT Ni will be etched faster than copper and you as you guess only gold will remine (on panel or in etching solution)

----- Original Message ----
From: Lin Leo <[log in to unmask]>
To: [log in to unmask]
Sent: Saturday, May 27, 2006 3:25:06 AM
Subject: [TN] Electrolytic Ni/Au in DES


Hi,

  Does anyone have experience on electrolytic Ni/Au(Au thickness: ca. 12~20 micro-incheses; Hard gold Au-Co alloy) acting as etching resist in DES(developing-CuCl2/HCl-stripping) process?  Does Au thickness have impact on etching solution attack?

  Thanks

  Leo


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
___________________________________________________  最新版 Yahoo!奇摩即時通訊 7.0,免費網路電話任
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
打!  http://messenger.yahoo.com.tw/

ATOM RSS1 RSS2