Hi Jeff,
You are  correct to worry about this. Non-symmetrical layups can be assemble,
but require special handling, in particular more extensive, and perhaps
depending on the severity of the non-symmetry unequal, pre-heating. The only
way to find out is to build some prototypes and assemble them fully loaded.
Make sure the prototype is build with the same material as would be the
product.

Werner Engelmaier
Engelmaier Associates, Inc.
Electronic Packaging, Interconnection and Reliability Consulting
23 Gunther Street
Mendham, NJ  07945  USA
Phone & Fax: 973-543-2747
E-mail: [log in to unmask] 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2