Werner ,
I understand the issues around not achieving a homogenous joint ie. >217C that is why I ran a profile peak of 232ish, which I would have thought would have been enough to provide a good joint but not high enough to cause problems with packages that are not rated for PbF.
Regards,
Iain.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: 20 November 2006 15:06
To: Braddock, Iain; [log in to unmask]
Subject: Re: [TN] BGA anomaly
*** WARNING ***
This mail has originated outside your organization,
either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
Hi Iain,
For a mixture of SnPb & PbF part (in particular PbF BGA's - SAC305) using a 63/37 SnPb solder, the preferred reflow profile is definitely a LF-SAC profile, NOT a SnPb-profile.
Werner
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|