TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Clayton Gardner <[log in to unmask]>
Date:
Tue, 13 Mar 2001 08:54:01 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Craig Hillman <[log in to unmask]>
Subject:
From:
Craig Hillman <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (86 lines)
Clayton,

What is the lead plating? Copper corrosion products, primarily sulfides and
chlorides (not oxides), have been known to migrate into the package as well
as migrate between leads (causing increased current leakage or an electrical
short). In order for migratory corrosion products to appear, you need
chlorides and sulfides in the environment. This can be from leftover fluxes
and other chemicals on the board or it can be from industrial gases (you'd
be suprised how much chlorine gas you breathe in everyday).

The corrosion products can only migrate into the package if there is a
delamination between the encapsulant and the lead. Have you conducted
acoustic microscopy of the component after reflow?

If you want to qualify the components, you will need to run them through a
typical solder reflow (with flux) and then subject it to either HAST or
mixed flowing gas (MFG). As a general rule of thumb, if your cleaning
process is thorough, your use environment is benign (controlled office) and
your required lifetime is less than five years, these imperfections should
not be a problem. However, if you have leftover flux on the board, you could
see leakage problems in as little as six months.

Craig


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Clayton Gardner
Sent: Monday, March 12, 2001 8:13 PM
To: [log in to unmask]
Subject: [TN] Exposed Copper


Hi All

Can you please comment on the following

Is there any associated/documented risk, if there are small plating
imperfections on copper leaded SO08 components leaving a small section of
exposed copper as the lead exits the component body??

We use IPC 610 Class 2 for this product.  Our customer has concerns about
the exposed copper leading to corrosion and entering the component body.

Any help or info you can provide would be muchly appreciated.

Thanks

Clayton Gardner
Engineering Manager
AEMS
11-13 Fiveways Blvd
Keysborough VIC  3173
AUSTRALIA

Ph 61 3 9701 5499
Fx 61 3 9701 5422

email: [log in to unmask]

web:  www.aems.net.au

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2