Had to solder to Cu-Ni terminal lugs at one time. The solderabilty was what I would call lousy. Since I had no restrictions on what I could use I dipped them in a Nitric acid solution and immediately tinned them. This worked ok. Also tried rubbing with a rubber eraser, the kind with abrasive in it. That worked but not as well. Both methods are pretty much frowned upon in electronics though.
-----Original Message-----
From: Glenn Pelkey [mailto:[log in to unmask]]
Sent: Friday, November 07, 2003 10:59 AM
To: [log in to unmask]
Subject: [TN] Cupron solderability
Hi folks,
Anyone familiar with Cupron and if it is solderable?
Checked Matweb, but no indication on solderability. Basically, it is a copper and nickel alloy, although some show an iron component. A quick test here with a sample showed no wetting action, even with an aggressive flux. There is no surface finish to protect the copper or nickel from oxidation.
Thanks,
Glenn
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|