TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 8 Oct 2008 14:15:06 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (147 lines)
Bi/Sn has long been a low MP alternative alloy for special situations.
Now that Pb containing surfaces have washed out of the system with move to
Pb-free, Bi based alloys are being more widely used when a low MP is needed.
The key is to use a low temperature flux to go with the low MP alloy. The
rate of joint formation is also slower due to  low tin content so the flux
has to be capable of sustaining a longer reflow time.
Finally many people favour use of an alloy with a small addition of Ag, this
makes the alloy more ductile 


Regards 

Mike Fenner 
Indium Corporation 

T: + 44 1908 580 400 
M: + 44 7810 526 317 
F: + 44 1908 580 411 
E: [log in to unmask] 
W: www.indium.com 
Pb-free: www.Pb-Free.com 

---------------------

Indium Corporation
Incorporated in New York, USA
Registered office: (Not for correspondence) 
77-97 Harpur Street, Bedford , UK
Registered number: fc16473


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Tuesday, October 07, 2008 10:13 PM
To: [log in to unmask]
Subject: Re: [TN] Sn-Bi Alloy for soldering

Amol,

In a prior life (or two), I tried soldering SnBi with hand soldering and
reflow soldering. My impression was that it did not wet well, despite the
lower melting point. At that time, if I had to select a Lead Free Solder, I
would not go with SnBi. 

However, that was several years ago and I have not tried it since then.
Assuming that the solder manufacturers increased the flux activity since, I
would consider it for non aerospace applications where I have heard that it
has been used successfully. Otherwise, I would not use it for high
reliability or aerospace applications, IMHO.

Hope this helps.

Good Luck.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Tuesday, October 07, 2008 11:57 AM
To: [log in to unmask]
Subject: [TN] Sn-Bi Alloy for soldering

Does anybody have any experience with Sn-Bi alloy used for soldering
lead-free boards? I am looking at literature available out there and see
Sn-Bi used as a surface finish for components, but I have not yet found a
reference where it is used for soldering.

Looking for pros/cons, good/bad experiences and things to look out for
during soldering.

The application is all SMT, with a temp sensitive part. The manufacturer
therefore wants to use Sn-Bi alloy as this is a lower melting point alloy

Regards,
Amol





WARNING:  Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government.  Transfer of such data by any means to
a foreign person, whether in the United States or abroad, without proper
export authorization or other approval from the U.S. Department of State is
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and protected
from disclosure under the law. Any unauthorized review, use, disclosure, or
distribution is prohibited. If you are not the intended recipient, please
contact the sender by reply e-mail, and delete/destroy

all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2