TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Herring <[log in to unmask]>, [log in to unmask]
Date:
Tue, 29 Jul 2014 09:44:03 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Subject:
From:
Dwight Mattix <[log in to unmask]>
Message-ID:
In-Reply-To:
<[log in to unmask] nics.com>
Content-Type:
text/plain; charset="us-ascii"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
yep, looks like ENIG is lifting over some of the filled vias.

At 09:23 AM 7/29/2014, Steve Herring wrote:
>It looks to me like their Screen Printer is doing a poor job of 
>under stencil wiping, leaving solder paste on the underside of the 
>stencil that gets transferred to the gold areas on the edge of the pcb.
>During reflow, the small balls of paste flow into nice circles.
>Not all stencil wiping paper is created equal.
>
>Steven E. Herring
>Engineering Manager
>Pennatronics
>75 Technology Drive
>California, Pa 15419-0638
>P 724-938-1800 x 214
>F 724-938-1809
>[log in to unmask]
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster
>Sent: Tuesday, July 29, 2014 12:13 PM
>To: [log in to unmask]
>Subject: [TN] Trying to figure out possible mechanism for contamination
>
>We have been seeing a problem recently on several different CCA'S 
>that we are having assembled.
>The boards are ENIG with plug and plate.  The assembly shop is 
>assuring us that these gold areas are being Protected during the 
>entire assembly process with kapton tape.
>I was thinking it was flux splatter since the areas are always 
>almost perfectly circular.
>The locations are very random and range from nothing to what is in 
>the picture.
>Is there any other mechanism that might be causing this? On our next 
>run I am going to go to the shop To witness the taping. But I was 
>curious if maybe it's some other cause.
>Mr. Gregory was kind enough to post a picture.
>http://stevezeva.homestead.com/spots.jpg
>
>Any thoughts would be appreciated
>Thank You
>John Foster
>L3 Communicatons
>
>Confidentiality Notice:  The information contained in this message 
>is intended only for the use of the addressee, and may be 
>confidential and/or privileged.  If the reader of this message is 
>not the intended recipient, or the employee or agent responsible to 
>deliver it to the intended recipient, you are hereby notified that 
>any dissemination, distribution of copying of this communication is 
>strictly prohibited.  if you have received this communication in 
>error, please notify the sender immediately.
>
>Warning: This document may contain technical data within the 
>definition of the International Traffic in Arms Regulation (ITAR) 
>and is subject to the export control laws of the U.S. 
>Government.  Transfer of this data by any means to a foreign person, 
>whether in the United States or abroad, without an export license or 
>other approval from the U.S. Department of State, is strictly prohibited
>
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud service.
>For more information please contact helpdesk at x2960 or 
>[log in to unmask] 
>______________________________________________________________________
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud service.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2