At first glance it appears that pores in the gold are exposing the underling
nickel/copper to a constituent of the tape (or contaminant) released at
temperature.
On 7/29/2014 12:12 PM, John Foster wrote:
> We have been seeing a problem recently on several different CCA'S that we are having assembled.
> The boards are ENIG with plug and plate. The assembly shop is assuring us that these gold areas are being
> Protected during the entire assembly process with kapton tape.
> I was thinking it was flux splatter since the areas are always almost perfectly circular.
> The locations are very random and range from nothing to what is in the picture.
> Is there any other mechanism that might be causing this? On our next run I am going to go to the shop
> To witness the taping. But I was curious if maybe it's some other cause.
> Mr. Gregory was kind enough to post a picture.
> http://stevezeva.homestead.com/spots.jpg
>
> Any thoughts would be appreciated
> Thank You
> John Foster
> L3 Communicatons
>
> Confidentiality Notice: The information contained in this message is intended only for the use of the addressee, and may be confidential and/or privileged. If the reader of this message is not the intended recipient, or the employee or agent responsible to deliver it to the intended recipient, you are hereby notified that any dissemination, distribution of copying of this communication is strictly prohibited. if you have received this communication in error, please notify the sender immediately.
>
> Warning: This document may contain technical data within the definition of the International Traffic in Arms Regulation (ITAR) and is subject to the export control laws of the U.S. Government. Transfer of this data by any means to a foreign person, whether in the United States or abroad, without an export license or other approval from the U.S. Department of State, is strictly prohibited
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
--
Bhanu Sood
Center for Advanced Life Cycle Engineering (CALCE)
Test Services and Failure Analysis Laboratory
Room 0128, Glenn L. Martin Hall (Building 088)
University of Maryland
College Park, MD 20742
Tel: +1 (301) 405 3498
Fax: +1 (301) 314 9269
e-mail: [log in to unmask]
Skype: calce_umd
website: www.calce.umd.edu/TSFA
Confidentiality Notice: The information contained in this e-mail
and any attachments may be legally privileged and confidential.
If you are not an intended recipient, you are hereby notified that
any dissemination, distribution or copying of this e-mail is strictly
prohibited. If you have received this e-mail in error, please notify
the sender and permanently delete the e-mail and any attachments
immediately. You should not retain, copy or use this e-mail or
any attachment for any purpose, nor disclose all or any part of the
contents to any other person.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|