Hi Carl. I would consider that the arsenic remaining from the plating process is the result of poor cleaning. As a result the arsenic caused oxidation of the Sn of the plating which is a common problem for solderability problems on Sn/Pb which is usually very easy to solder.
----- Original Message -----
From: Carl Ray
To: [log in to unmask]
Sent: Tue, 8 Jun 2010 18:44:21 +0000 (UTC)
Subject: [TN] Arsenic from XRF Testing
All,
I have a question. We were seeing some solderability issues with some components that were provided by our customer. These devices were Sn-Pb over Cu plating per the data sheet. We tested 3 samples and noticed where all three samples have very high concentration of Arsenic. Some as much 4-5%. What could possibly be the cause for this? I understand Arsenic is used during plating process but I did not think it was as significant as 4-5%.
Carl Ray
Staff Engineer
Teledyne Electronic Manufacturing Services
1425 Higgs Rd.
Lewisburg, TN 37091
Direct: 931-270-2724
Cell: 931-637-5958
Email: [log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|