TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Tom Oliver <[log in to unmask]>
Date:
Thu, 26 Aug 1999 11:03:12 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Oliver <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Hello
My first post and first question to the experts.
I am new to the electronic game most of my experience has been in mechanical
inspection and test.
My question: is there a rule of thumb on material shrinkage on board
material or a spec. Our boards are coming in with all the dimensions at
nominal but after wave they have shrunk down to the low limit and sometimes
below low limit. Most of our tolerances are +/- .003.
This is giving us headaches with interference problems when we put other
components on the boards.
Is it normal for the boards to shrink. Our arrays are approx. 4" x 12" with
25 separate boards on each array.
Thx's in advance
Tom Oliver
Eagle Comtronics
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2