At 09:03 AM 12/31/96 PST, you wrote:
>     I would like to know the causes of solder blow-out in soldered PTH 
>     assemblies other than the insufficient copper thickness of PTH. 
>     We are encountered this kind of soldering problem on PCB with 
>     0.8mil(average) in PTH copper thickness.
>     Any help to identify the problem would be highly appreciated
>     
>     Best Regards,
>     
>     KP Chan
>     Email: [log in to unmask]
>
>********************************************************************

Hi Chan,

I ever encounter this issue before. Even the drilling and plating are good,
I still
faced this problem. 
I understand the raw material used for PCB fabrication is one of the
culprits. 

Try cleaning and later bake the board at 100 deg. C for 4 hrs.

Good Luck..

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2