Steve, Joe
General purpose RTV (RTV-108) releases an Acid Acid during cure
and corrodes copper, brass and sensitive metals. It is therefore NOT for
use in delicate electrical or electronic applications. However, there is an
electrical grade RTV (RTV-162) made by GE Silicones, General Electric Co.,
Waterford NY, 12188 518-237-3330. We have used this product for many
years and have experienced no problems.
Tom Cooper
TTC
"<Joseph M. Webb>" <"Joseph_M_Webb/ElecTec/Teledyne"@TELEDYNE.COM> on
03/11/99 09:17:23 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Joseph_M_Webb/ElecTec/Teledyne"@TELEDYNE.COM
To: [log in to unmask]
cc:
Subject: Re: [TN] RTV for SMT components
Steve,
Room Temperature Vulcanizing silicone.
I could not venture a source for the material that would be appropriate for
your use.
A word of caution though - I have a recollection of a very good friend of
mine (Hello Gene!) telling me that these materials become conductive at
high frequencies. I through this out there for what it is worth!
Joseph Webb
TET/Halco
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|