TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Tom Cooper <[log in to unmask]>
Date:
Thu, 11 Mar 1999 10:36:20 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (68 lines)
Steve, Joe
           General purpose RTV (RTV-108) releases an Acid Acid during cure
and corrodes copper, brass and sensitive metals. It is therefore NOT for
use in delicate electrical or electronic applications. However, there is an
electrical grade RTV (RTV-162) made by GE Silicones, General Electric Co.,
Waterford  NY,  12188  518-237-3330. We have used this product for many
years and have experienced no problems.

Tom Cooper
TTC





"<Joseph M. Webb>" <"Joseph_M_Webb/ElecTec/Teledyne"@TELEDYNE.COM> on
03/11/99 09:17:23 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to "Joseph_M_Webb/ElecTec/Teledyne"@TELEDYNE.COM

To:   [log in to unmask]
cc:
Subject:  Re: [TN] RTV for SMT components




Steve,

Room Temperature Vulcanizing silicone.

I could not venture a source for the material that would be appropriate for
your use.

A word of caution though - I have a recollection of a very good friend of
mine (Hello Gene!) telling me that these materials become conductive at
high frequencies. I through this out there for what it is worth!

Joseph Webb
TET/Halco

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2