TECHNET Archives

September 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Datacom - Juliano Ribeiro <[log in to unmask]>, [log in to unmask]
Date:
Wed, 16 Sep 2015 09:12:22 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<005c01d0f080$bdda12d0$398e3870$@ribeiro>
MIME-Version:
1.0
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (58 lines)
The "magic" Number should stay the same 1-3 micron but you'd also have to keep an eye on what happened to the layer of E-Ni underneath.

Regards,

Vladimir

SENTEC

Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message  
From: Datacom - Juliano Ribeiro
Sent: Wednesday, September 16, 2015 09:09
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] BGA Reworked Intermetalic

Hi to all,



When we reworked the BGA, removed the component of the board and replacement
another BGA, what’s the intermetalic thickness ideal after the rework?



p.s: Our pcb is ENIG finished and the solder is Tin Lead.



_____________________________

Juliano Bettim Ribeiro

DATACOM 

ENGENHARIA DE PROCESSOS 
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000 
+55 (51) 8446-2135

+55 (51) 3933-3000 

Ramal: 3484
<mailto:[log in to unmask]> [log in to unmask] 
<http://www.datacom.ind.br/> www.datacom.ind.br




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2