My understanding is that the matte tin finishes do not eliminate tin
whisker. Some argue that the finish reduces the length of the whiskers
that are likely to form. I wish I had ready access to the presentations
that I have seen on this subject. Let's see where this thread goes.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gaby Bogdan
Sent: Monday, January 27, 2003 1:36 AM
To: [log in to unmask]
Subject: [TN] Tin whiskers
After storage of about 6 months we saw Tin whiskers inside the hole
barrel on Immersion Tin plated boards. It is the second time we found
them, and the batches were from two different suppliers.
According to our knowledge, they they are using the immersion tin
technologies which are said to prevent whisker formation when applied
properly.
What can be the cause?
Gaby
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|