Yes. You are correct. Sometimes the panelization scheme can induce
warpage that disappears after singulation (or becomes worse).
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Tuesday, July 14, 2009 11:03 AM
To: [log in to unmask]
Subject: Re: [TN] Maximum Allowable Bow & Twist for Post T/C Reliability
Hi Richard,
I know you quoted the spec but I don't understand why you would measure
multiple boards in panel form. It seems to me that if you had an array
that
had large tab-route edges and spacers in between the boards that
additional
area could give you a bow or twist that exceeds the allowable limits but
the
individual boards could be OK.
I'm I missing something here?
KennyB
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Tuesday, July 14, 2009 8:50 AM
To: [log in to unmask]
Subject: Re: [TN] Maximum Allowable Bow & Twist for Post T/C Reliability
I understand now what you mean.
IPC-6012B states the following on bow and twist:
3.4.3 Bow and Twist Unless otherwise specified in the
procurement documentation, when designed in accordance
with 5.2.4 of IPC-2221, the printed board shall have a
maximum bow and twist of 0.75% for boards that use surface
mount components and 1.5% for all other boards. Panels
which contain multiple printed boards which are
assembled on the panel and later separated shall be
assessed in panel form.
Bow, twist, or any combination thereof, shall be determined
by physical measurement and percentage calculation
in accordance with IPC-TM-650, Method 2.4.22.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|