TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wtBZf-000Bj9C; Tue, 29 Jul 97 07:40 CDT
Old-Return-Path:
Date:
Tue, 29 Jul 1997 08:54:07 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Mailing-List:
<[log in to unmask]> archive/latest/14372
TO:
Mime-version:
1.0
Return-Path:
<TechNet-request>
X-Loop:
From [log in to unmask] Thu Jul 31 11:
44:20 1997
Resent-Message-ID:
<"kHzv93.0.TkJ.sIUtp"@ipc>
Content-type:
text/plain; charset="us-ascii"
Subject:
From:
GeoFranck <[log in to unmask]>
Content-transfer-encoding:
7bit
Message-Id:
X-Mailer:
Microsoft Internet Mail & News for Macintosh - 3.0a (370)
>From willli Tue Jul 29 07:
40:40 1997
Parts/Attachments:
text/plain (31 lines)
Hello Colleagues
One of my favorite 'smaller-is-better' design Engineers found a Nanionics
connector which uses 30 AGW wire for thru-hole leads, and recommends a thru
hole diameter of 12-16 mils.  (Tight tolerance, too, huh?)
Question:  Has anyone had problems with soldermask being left in these small
holes.  The alleged failure mode is from the LPI-developer not able to
develop out soldermask in these holes, due their small diameter.  This is
reasonable, since LPI developing likes alot of impingement.
I am looking for individuals who can commiserate, and who may have worked
out an alternative.
Other topic we could also talk about is holding a +/- .002 hole size with
solder coating; HASL?; Plate and reflow?; Ni/ Immersion Gold?


Finally, who in the Board industry told Nanionics this was an 'easy' thing
to do?  (just kidding)

George Franck
Raytheon E-Systems

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2