TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"WEEKES, MICHAEL HS-SNS" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 4 Aug 2003 12:54:23 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (209 lines)
awesome,

Mike Weekes
Hamilton Sundstrand
815 394 2497

thanks, a million.

Michael Weekes
Master Engineer - EOE
Hamilton Sundstrand / UTC
MS 190-6
4747 Harrison Ave. PO Box 7002
Rockford, IL 61125-7002
815 394 3362
[log in to unmask]


-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, August 04, 2003 11:30 AM
To: [log in to unmask]
Subject: Re: [TN] commercial resistors and capacitors in high-rel mil
applications


Michael,

A Rockwell-Collins military radio, ARC-210, was the first to be procurred
under the Navy's "Aquisition Reform/Mil Spec Streamling" program.  There is
a write-up in the January 1997 "Signal" magazine.  I can fax you a copy if
you need it right away.

We have been using commercial Rs & Cs for about 8 years without any issues.

Jim Carlson
Rockwell Collins Reliability Engineer



                      "WEEKES, MICHAEL
                      HS-SNS"                  To:
[log in to unmask]
                      <[log in to unmask]        cc:
                      TC.COM>                  Subject:  [TN] commercial
resistors and capacitors in high-rel mil applications
                      Sent by: TechNet
                      <TechNet@listserv
                      .ipc.org>


                      08/04/2003 10:05
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      "WEEKES, MICHAEL
                      HS-SNS"






I have been asked to see if there are any papers or success stories out
there for MIL or avionics manufacturers or assemblers who have successfully
replaced expensive "qualified" mil-type resistors and capacitors  with
less-costly, yet as-reliable resistors or capacitors to meet the needs of
customers like Lockheed Martin, Boeing or Airbus?  I'm looking for anything
that can be shared from the component manufacturer, electronics assembler
or
end customer perspective.
This is urgent.

thank you,
Mike Weekes
[log in to unmask]
815 394 3362

Michael Weekes
Master Engineer - EOE
Hamilton Sundstrand / UTC
MS 190-6
4747 Harrison Ave. PO Box 7002
Rockford, IL 61125-7002
815 394 3362
[log in to unmask]


-----Original Message-----
From: Steve MacDonald [mailto:[log in to unmask]]
Sent: Monday, August 04, 2003 9:51 AM
To: [log in to unmask]
Subject: Re: [TN] Score to trace criteria


Hi Frank.

I actually wrote one based on the design spec references to I/L clearances
and our own manufacturing requirements. The 2221 design spec states that a
recc. min trace to edge clearance of .0157 inches be maintained on I/L with
additional spacing on outerlayers based on fab and assembly considerations.

(Our considerations) (W/ IPC-A-600 allowance of .098 inches of edge nicks
or
haloing as a guide)
We adjusted our figures for worst case (scored edge):  +/- .002 for A/W
registration.  +/- .002 for drill registration. If taking score you need up
to .0125 inches from center score for blade width and depth of cut and
another .003 inches for blade wander. (the score line can easily be up to
.....025 in. wide.

So we set optimum safe distance on outers (from score centerline to nearest
feature) of .035 inches.  Routing allows you to decrease that by the score
adjustments.  Customers are notified when the supplied data violates that
and they may opt to allow a change or accept as it.  We record and file
their response for future reference.

This doesn't apply to heatsinks, ground shields or edge connectors of
course.  And better equipment begets tighter allowances so as we change
equipment we will adjust our house spec accordingly.


Hope this helps.

Steve MacDonald

----- Original Message -----
From: "Franklin D Asbell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, August 04, 2003 09:42
Subject: [TN] Score to trace criteria


> Is anyone aware of written criteria dealing with scored edge to trace
edge
> criteria??? design criteria??? specification tolerance, etc etc
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2