Siggi: The Probimer 65 has more of a "lime" or slightly yellow-green color.
Somewhat similar to Probimer 52. The 77 has a "medium" green color. It's a
little hard to distinguish between the two. However if you look at them side
by side with the same type of background i.e. mask over laminate or mask
over groundplane you should be able to see the difference.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Zweigart, Siegmund [mailto:[log in to unmask]]
Sent: Wednesday, March 05, 2003 7:34 AM
To: [log in to unmask]
Subject: [TN] Probimer 65 - Probimer 77
Hello
Is there a possibility to see (or a simple analyses method) on a occupied
board if the soldermask is based on Probimer 65 or Probimer 77?
-- I know both are green, but maybe one is more green than the other?
Thanks for your help
Siggi
> ____________________________
>
> Best Regards /
> Mit freundlichen Grüssen
>
> Dr. Siegmund Zweigart
>
> New Technology Manager
>
> Solectron GmbH
> Solectronstr. 2
> 71083 Herrenberg, GERMANY
>
> * +49 (0) 7032 998-194
> * +49 (0) 7032 998-49-194
>
> mailto:[log in to unmask]
www.solectron.com
> _____________________________________
>
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|