Siggi: The Probimer 65 has more of a "lime" or slightly yellow-green color. Somewhat similar to Probimer 52. The 77 has a "medium" green color. It's a little hard to distinguish between the two. However if you look at them side by side with the same type of background i.e. mask over laminate or mask over groundplane you should be able to see the difference. Regards Michael Barmuta Staff Engineer Fluke Corp. Everett WA 425-446-6076 -----Original Message----- From: Zweigart, Siegmund [mailto:[log in to unmask]] Sent: Wednesday, March 05, 2003 7:34 AM To: [log in to unmask] Subject: [TN] Probimer 65 - Probimer 77 Hello Is there a possibility to see (or a simple analyses method) on a occupied board if the soldermask is based on Probimer 65 or Probimer 77? -- I know both are green, but maybe one is more green than the other? Thanks for your help Siggi > ____________________________ > > Best Regards / > Mit freundlichen Grüssen > > Dr. Siegmund Zweigart > > New Technology Manager > > Solectron GmbH > Solectronstr. 2 > 71083 Herrenberg, GERMANY > > * +49 (0) 7032 998-194 > * +49 (0) 7032 998-49-194 > > mailto:[log in to unmask] www.solectron.com > _____________________________________ > > > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------