Apart from Mike's & Frank's ; Doug, let's take the work personally :

Imagine the 2M picture :
There is Doug, justly frrreshly pooped from clean bath , ready for drying .
Presses button ; comes out AN AIR GUN ,
which with the below mentioned deafening noise commences it's task with
pitiful efficiency and truckloads of entailed negatives .
Happy ? No ?

Ok , lets have 3M picture :
As above , Doug whistles high C voice command , and, viola, the LARGE DIA
CENTRIFUGE WITH FILTER,
aka common kitchen window fan , with variable speed to validate the optimal
VOLUME flow,
commences it's task .
Doug is dry in seconds (60 of 'em), ready for his favorite "watering" hole .

"do not to others you'd whish not to yourself"

amen

PS
yes emitting needle spicing the air with occasional ozone molekule won't
hurt.
Desist the lavender oil capillary .


-----Original Message-----
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Friday, 10 March 2000 7:53
To: [log in to unmask]
Subject: Re: [TN] High Pressure Air Dry for PWBs - creates ESD?


In a message dated 3/9/00 1:47:13 PM Eastern Standard Time,
[log in to unmask] writes:

> Our current method of drying PWBs after cleaning is to blow them dry with
a
>  standard air gun with up to 125 psi of air.  Other than the sound level
>  which can be deafening does this create an ESD problem with static
generated
>  by the fast moving air?  What are the best methods of noise and static
>  abatement?
>

I would be far more concerned about the oil and other contaminants you are
blowing onto the assembly.

Doug Pauls

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2