Good Morning Keith,
The easiest solution is to create a note on your drawing that states the
maximum lead protrusion shall not exceed .xxx". The drawing requirments
take precedence over any referenced standard unless otherwise stated in
contractual documentation with your customers.
The additional drawing note can limit the applicability of the "excess" lead
protrusion by stating "for leads of U1-U4, S1" etc.
Steve Sauer
Mfg Engineer
Northrop Grumman, Xetron
-----Original Message-----
We are having a vigorous discussion about how to deal with lead
protrusion on our thru hole boards. We build mainly IPC class 3 boards,
Our area of concern is DIP packages along with sockets, and
connectors. When we insert DIPs we clinch two opposing corner pins,
connectors and sockets are retained with temporary solder mask (goop).
we are finding that the leads on these parts tend to exceed the max lead
protrusion permitted for class 3 boards when used in .06 nominal
thickness boards, but do not want to get into the quagmire of trimming
leads and inspecting or reflowing after trimming. These boards will
meet the class 2 requirements, and there is no danger of violating the
minimum electrical spacing requirements when these boards are installed
in our systems.
Anyone else having this problem? If so, how did you resolve it? Your
support is greatly appreciated.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|