TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Thu, 31 Oct 2002 08:34:28 -0500
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Graham Collins <[log in to unmask]>
Subject:
From:
Graham Collins <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (74 lines)
Hi Keith
We build some similar stuff.  You have two options other than the hand trimming:

Run the DIP packages through a forming and trimming machine, to trim the leads to an acceptable length.  This is typically what we do, so we end up with enough lead that the CS-400 can crimp it but not too much for protrusion.

Alternatively - have a drawing note added to increase the allowable lead length to 90 thou or whatever is reasonable in the applications you have.  The drawing note overrules the IPC requirement, so you are in the clear.   



regards,

Graham Collins
Process Engineer, 
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215

>>> [log in to unmask] 10/31/02 09:04AM >>>
We are having a vigorous discussion about how to deal with lead
protrusion on our thru hole boards.  We build mainly IPC class 3 boards,

and have two Contact Systems CS400-D thru hole insertion machines that
we use to populate these boards.  Discrete parts are not a problem, as
the leads are crimped to retain the parts in the boards for wave
soldering.  Our area of concern is DIP packages along with sockets, and
connectors.  When we insert DIPs we clinch two opposing corner pins,
connectors and sockets are retained with temporary solder mask (goop).
we are finding that the leads on these parts tend to exceed the max lead

protrusion permitted for class 3 boards when used in .06 nominal
thickness boards, but do not want to get into the quagmire of trimming
leads and inspecting or reflowing after trimming.  These boards will
meet the class 2 requirements, and there is no danger of violating the
minimum electrical spacing requirements when these boards are installed
in our systems.

Anyone else having this problem?  If so, how did you resolve it?  Your
support is greatly appreciated.


  Keith Calhoun
  Manufacturing Engineer
  Sierra Research, an Integrated Defence Technologies company
  485 Cayuga Road PO Box 222 Mail Stop 334
  Buffalo
  New York
  14225
  USA
                                         Fax: (716)631-7849
                                        Work: (716)631-6434
                                        <[log in to unmask]>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2