Hi Lenny
The NanYa and Isola material is certainly in the same family of materials
so by large i would say they are comparable.
There could be a possibility that 406 gives off slightly less smoke when
burning, this is not part of the specification but your customer could
have tested several different materials for this reason.
A comparison test between the to materials on the same smoke desity test
equipment might give you an indication.
BR
Grunde
Lenny Carter <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
24.04.2008 00:00
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Smoke Desnity test, FR4-06 \ NP-170R
Howdy tech-netters, A while back we had a customer requesting FR4-06 pcb
material and one of our pcb vendors asked to use their manufacturer's
equivalent NP-170R instead. We approved it's use.
Recently a customer said our assemblies are failing a smoke density test.
One of our group members is suspecting the pcb material.
1) Could pcb material be related?
2) Is NP-170R a valid replacement for FR4-06?
Thanks,
Lenny Carter
Design Engineer
ERG, Inc.
ph (607) 754-9187 x3063
www.ergpower.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|