TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Tue, 4 May 2010 18:21:09 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (88 lines)
Reference in 80s may have some discussion about it.  If the mask is not cured properly or difficult to cure, you will have solderballs (non wetting characteristic of mask is not developed). 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Louis Hart [mailto:[log in to unmask]]
Sent: Tuesday, May 04, 2010 04:54 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Does solder mask specified create solder balls?

Don, A book I have from 1998, Failure Modes and Mechanisms in Electronic Packages, by Viswanadham and Singh, addresses solder balling in a few pages. (At least one of these gentlemen was a Technetter about 10 years ago, I believe.) Among their observations, glossy mask is said, supported by  a reference, to promote solder ball formation.

Louis Hart

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Don McFarland
Sent: Tuesday, May 04, 2010 4:20 PM
To: [log in to unmask]
Subject: [TN] Does solder mask specified create solder balls?

Hi Technetters, 

I was asked to perform a DOE to determine if there was a correlation
between solder mask types and the rate at which we see solder balls
develop on the PWB surface. I searched through the archives and found a
few articles from the mid-90s about this topic, but couldn't glean
anything exciting from the posts reviewed. I am wondering if anyone knows
of a good source of information that addresses this topic or has anything
that would be useful for us. 

We have made a number of changes to other process variables (e.g. stencil
apertures, solder pastes, paste viscosity, profiles, etc) and have seen
good results, but we wanted to rule this out as a causal factor as well. 

Any help is greatly appreciated!

Don McFarland
  

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2