TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 29 Jun 1998 11:05:06 +0000
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Benedicto Cruz <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
7BIT
From:
Benedicto Cruz <[log in to unmask]>
Comments:
Authenticated sender is <bcruz@[192.1.1.215]>
Parts/Attachments:
text/plain (36 lines)
Hi everyone,

I am using an epoxy dispensing machie that performs potting on metal
scases. One of my biggest problem is the occurrence of bubbles after
dispensing.
The machine has its own vacuum for the chemicals before mixing. But
the dispensing stage is done on room parameters. Bubbles occur before
and after oven curing.
Can this occurrence of bubbles be controlled? Or to we need a vacuum
verger during dispense?

I would also like to ask for the standard soldering iron temperature
used for rigid PCBs and flex PCBs.


 Regards.

Jon Cruz
OIC Supervising Product Engineer
Electronic Assemblies Inc.
[log in to unmask]
tel.# 823-7317/7593884
fax# 8238326

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2