In a past life we used brass shields that were tin/lead plated.  They were
a few mils thick and were etched and with forming grooves for the operator
to bend at installation.  This worked very well and never had a soldering
problem.



                    Earl Moon
                    <[log in to unmask]       To:     [log in to unmask]
                    .COM>                cc:
                    Sent by:             Subject:     Re: [TN] RF Shield Plating
                    TechNet
                    <[log in to unmask]
                    RG>


                    01/15/02 11:24
                    AM
                    Please respond
                    to "TechNet
                    E-Mail
                    Forum.";
                    Please respond
                    to Earl Moon






Dan,

Can't thank you enough. I'm sure Peter thanks you as well. His problems
seems a bit different with the Ni finish. Any suggestions?

The German silver thing occurred using shields on R/F filters. It happened
several times so I contacted someone at HAC and they recommended the "pink
death" flux that did the job but not without regrets.

Thanks again,

Earl Moon

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2