TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Strathie <[log in to unmask]>
Date:
Thu, 24 Jul 2008 14:51:46 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (70 lines)
IF you are cleaning a solvent (resin) based flux you will be using a
chemical in the first wash stage. This chemical makes the flux water
washable, you  then water rinse as required. Final rinse should be DI so as
to leave no conductives on work.
If you switch to a water washable flux, you dispense with the first stage
chemical, everything else stays same.

Regards 

Mike Fenner 
Indium Corporation 

T: + 44 1908 580 400 
M: + 44 7810 526 317 
F: + 44 1908 580 411 
E: [log in to unmask] 
W: www.indium.com 
Pb-free: www.Pb-Free.com 

---------------------

Indium Corporation
Incorporated in New York, USA
Registered office: (Not for correspondence) 
77-97 Harpur Street, Bedford , UK
Registered number: fc16473


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Strathie
Sent: Thursday, July 24, 2008 2:03 PM
To: [log in to unmask]
Subject: [TN] De-ionised water wash

We have been asked to look at replacing our water wash cycle in our lead
free assembly process with a de-ionised wash.  
I thought de-ionised wash had become redundant with water soluable fluges.
Deos anyone have any recomendations ?

Regards
Richard

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2