TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Tremmel <[log in to unmask]>
Date:
Wed, 8 Jun 2005 14:07:06 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
John Burke <[log in to unmask]>
Parts/Attachments:
text/plain (62 lines)
That depends on a number of factors including the device weight vs the
number of connections, coplanarity of the package when the solder solidifies
etc.

John
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of David Tremmel
Sent: Wednesday, June 08, 2005 2:00 PM
To: [log in to unmask]
Subject: [TN] Solder Sphere Diameter


Technetters:

If a BGA has a pad of 20 mil and a solder sphere of 30 mil, what is the
diameter of the solder sphere after it has been soldered to the BGA?


David

_________________________________________________________________
Visita MSN Latino Entretenimiento: ¡música, cine, chismes, TV y más...!
http://latino.msn.com/entretenimiento/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2