Hi Ed! The Specific Heat Capacity of Sn60/Pb40 is 150 J Kg(superscript: -1)
K(superscript: -1) and the its Latent Heat of Fusion is 37 KJ Kg
(superscript: -1). You should be able to make your calculation using these
values plus don't forget to add into the equation the solderpot specific
heat contribution. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Ed Popielarski <[log in to unmask]>@ipc.org> on 10/07/2002 10:56:25 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Ed Popielarski <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Solder melt energy coefficient
Hi all,
Does anyone know the energy (BTU, Watts, HP, etc.) required to raise some
amount of SN63 solder (lbs, kg, etc.) some thermal unit (deg. F or C) in
an amount of time (min, hours, etc.)? Now to make the question even more
"anal" (pardon my moonish term) how about the energy to go through phase
transition? Have I been thinking about wave soldering too much? Probably
so, but I need this info to determine the correct kW values to heat an "N
lbs" pot in "X" time (a customer requirement).
Regards,
Ed Popielarski
QTA Machine
10 Mc Laren, Ste
Irvine, Ca. 92618
Phone:949-581-6601
Fax: 949-581-2448
Cel: 949-337-2578
WWW.QTA.NET
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|