Hi Ramon! The use of a solder/gold finish interface for connectors is not
preferred. A solder/gold finish interface is typically only used when: a)
the connection is a once or twice insertion for its life; b) high insertion
forces are employed to insure good metal-to-metal contact. The oxides of
tin and lead are not coherent, adherent species so they tend to "spall" off
creating connector debris that causes intermittent problems.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Dehoyos, Ramon" <[log in to unmask]>@ipc.org> on 10/09/2002
01:27:56 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Dehoyos, Ramon" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Golden Pin Connectors
If the pins of two gold Plated mating connectors were tinned,
would
it cause any intermittent connection in the future by the pins being
tinned
and the sockets being gold plated? Or would the connectors conduct just
fine?
Regards,
Ramon
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|