Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, stephengregory5849 <[log in to unmask]>
Date:
Mon, 27 Nov 2006 13:25:46 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
A<000e01c71248$beffaa00$09f39804@nem6v3iq5opkfv>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (125 lines)
Can't tell a lot from a single picture, but that little spur on the side
of the solder joint makes me think someone is doing solder touchup
without benefit of flux. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of stephengregory5849
Sent: Monday, November 27, 2006 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering Anomaly

Hi Everyone!

Well, I finally got Pat's picture up! The reason it's taken me so long
is because I'm back home in North Carolina, and the only internet access
I have is dial-up at a screaming 26.4 KB per second! I remember not that
long ago that was fast. But once you get used to a DSL or T1 connection,
well that's just dog slow.

Anyways, here's Pat's picture:

http://www.stevezeva.homestead.com/files/solder_anomaly2.JPG

To me that doesn't look right. I've soldered with a Sn62/Pb36/Ag2 paste
before and soldered lead-free components on a ENIG board and the joints
didn't look that rough. That's more than just cooling lines IMHO...

-Steve Gregory-

----- Original Message -----
From: "Diamond, Pat" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, November 27, 2006 2:12 AM
Subject: [TN] Soldering Anomaly


> Hi Technetters,
>
> We have recently received some assembled boards from a new supplier 
> and upon carrying out a First Article Inspection on them I noticed 
> what I thought were disturbed solder joints.  I then referred to 
> IPC-610 which seemed to confirm this.  Upon talking to the supplier 
> about this problem they said that this was not disturbance but 
> "cooling lines" due to the fact that the component leads were 
> lead-free and the solder paste was Sn62/Pb36/Ag2.
> They referred me to IPC-610 Para. 5.2.7 Fig. 5.56 (page 5-18) which 
> looks nothing like the joints on our components.  The only area this 
> anomaly is occurring is on the SOT 23 Transistors & Diodes.
> Our company is not a main line SMT producer and I have never seen this

> anomaly before.
>
> I have contacted Steve Gregory and he has kindly agreed to post a 
> couple of pictures on his website for me, see what you think.
>
> I really hope they are cooling lines!!!
>
> Thanks in advance for any help/advice you can offer.
>
> Best regards,
>
> Pat
>
>
> **********************************************************************
> ******
> ***************
> The information transmitted is intended only for the person or entity 
> to which it is addressed and may contain confidential and/or 
> privileged material.
>
> Any review, retransmission, dissemination or other use of, or taking 
> of any action in reliance upon, this information by persons or 
> entities other than the intended recipient is prohibited. If you 
> received this in error, please contact the sender and delete the 
> material from any computer.
> **********************************************************************
> ******
> ***************
> Mr Pat Diamond
> Senior Specialist Engineer
> Weston Aerospace                Tel:     +44 (0)1252  868122
> 124 Victoria Road               Fax:    +44 (0)1252 370298
> Farnborough, Hampshire, GU14 7PW        Web    www.westonaero.com>
> England         Email  mailto:[log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
> http://listserv.ipc.org/archives Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2