TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Carl VanWormer <[log in to unmask]>
Date:
Wed, 6 Apr 2005 08:16:52 -0700
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Carl VanWormer <[log in to unmask]>
Parts/Attachments:
text/plain (79 lines)
I'm using two versions of that package.  One is a single LED, while the
other is a dual LED.  Both use the same footprint, but the dual uses the
middle connection.  The center pad does seem to help with the centering.


Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR  97006
Phone (503)-617-7447    Fax (503)-617-6550



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: Wednesday, April 06, 2005 6:56 AM
To: [log in to unmask]
Subject: [TN]


Morning Everyone!

I just ran an assembly here that has some strange little right angle LED's
that I've never seen before. They were brought to my attention because many
of them were coming out of reflow pretty badly skewed. I've got a few images
of the LED at;  http://www.stevezeva.homestead.com

Look at "LED Top, LED Bottom, LED Pad Layout, and Recommended Layout".

For one thing, you'll see that these LED's have no real termination to
solder to, except on the face of the ends. Another thing I discovered after
I went and checked the dimensions of the pad layout in the gerbers, then
compared it with the manufacturers recommendation, the layout isn't even
close to what's recommended.

My question is, what would you do to try and protect what little solder
joint that is going to form, from being damaged? Some sort of glue bonding?

These little guys will need to withstand HASS testing in the upper-level
assembly believe it or not. But I'm not holding out much hope for that.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver this
message to anyone.  In such event, you should destroy the message and kindly
notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2