TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Wed, 6 Apr 2005 12:45:25 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (94 lines)
        Hi Ioan:
                        Can they be tacked with an adhesive?
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Tempea, Ioan
Sent: Wednesday, April 06, 2005 10:15 AM
To: [log in to unmask]
Subject: Re: [TN]


Steve,

we are soldering tons of these every day, with no issue. And they do not skew, maybe because the design has the middle pad (centering board). They wet properly, but I am only talking of commercial grade products that only see burn-in.

And an NTC solution for your problem, if you want them on the board after HASS, solder them manually after HASS...

Regards,
Ioan

> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Stephen Gregory
> Sent: Wednesday, April 06, 2005 9:56 AM
> To:   [log in to unmask]
> Subject:      [TN]
> 
> Morning Everyone!
> 
> I just ran an assembly here that has some strange little right angle LED's
> that I've never seen before. They were brought to my attention because
> many of them were coming out of reflow pretty badly skewed. I've got a
> few images of the LED at;  http://www.stevezeva.homestead.com
> 
> Look at "LED Top, LED Bottom, LED Pad Layout, and Recommended
> Layout".
> 
> For one thing, you'll see that these LED's have no real termination to
> solder to, except on the face of the ends. Another thing I discovered after
> I went and checked the dimensions of the pad layout in the gerbers, then
> compared it with the manufacturers recommendation, the layout isn't even
> close to what's recommended.
> 
> My question is, what would you do to try and protect what little solder
> joint
> that is going to form, from being damaged? Some sort of glue bonding?
> 
> These little guys will need to withstand HASS testing in the upper-level
> assembly believe it or not. But I'm not holding out much hope for that.
> 
> Kind regards,
> 
> -Steve Gregory-
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, Oklahoma
> (918) 459-2285
> (918) 459-2350 FAX
> __________________________________________________________________
> This message may contain information that is privileged and confidential to
> LaBarge, Inc.  It is for use only by the individual or entity named above.
> If you are not the intended recipient, you may not copy, use or deliver
> this message to anyone.  In such event, you should destroy the message and
> kindly notify the sender by reply e-mail.
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2