We have been having a problem with Dupont silver CB100 VIA Plug. The
boards are 12 layer, .062", FR4, Nickel/Gold plated.
We have a BGA pattern with VIA in hole. The VIAs are filled with CB100 VIA
plug and then the board is plated.
The VIAs are .010 causing an aspect ratio of 6.2:1. We are seeing after
solder reflow, inner layer delamination in the area of the
VIA filled BGA patterns. Has anyone seen this before? Does anyone use a
similar construction and had success? There are a few
theories flying around but I wanted to ask the IPC community for any
insight. Thank you in advance.
Best Regards,
Mike Forrester
Sr. Manufacturing Engineer
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|