TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 29 May 2001 16:48:40 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (139 lines)
Photo-imageable seems to be the most common, but there are the other types
around as well, and what I'm trying to find out is why would a designer
choose one type over another - are there any guidelines on which type to
select for particular sorts of applications or particular sorts of
substrate materials, and having chosen one, how does said designer
determine how thick it should be?

It's not left to the PCB fabricator, is it? I've heard enough to know that
too thick a resist layer can affect solderability among other things, while
too thin a layer reduces its effectiveness.

Put it another way - if I don't specify a resist and resist thickness, how
do I gain confidence that my PCB fabricator has chosen to put the right
thickness of the right resist on my boards? Any ideas?

Best regards

Pete





                    Paul Klasek
                    <PaulK@ResMed        To:     "[log in to unmask]" <[log in to unmask]>
                    .com.au>             cc:
                                         Subject:     RE: [TN] Which Solder Mask
                    05/29/01
                    01:33 PM






Thought it was bit fuzzy .
Photo-I is the way, watch for undercure (too fast process) on UV,
BLISTERS THAN . Common enough when fab's are stressed .
paul

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, May 29, 2001 3:05 PM
To: Paul Klasek
Subject: RE: [TN] Which Solder Mask



Thanks, Paul, but maybe I need to clarify what I'm after a bit - I'm
talking about the actual caoting that PCB fabricators put on boards to
cover external tracking, etc., the photo-imageable, dry film, UV cureable
type resist layer.

Pete Duncan




                    Paul Klasek

                    <PaulK@ResMed        To:     "'TechNet E-Mail Forum.'"
<[log in to unmask]>,
                    .com.au>             "[log in to unmask]"
<[log in to unmask]>
                                         cc:

                    05/29/01             Subject:     RE: [TN] Which Solder
Mask
                    06:17 AM









Multicore's "Spot Stik" latex used to behave well, easy peel afterwards,
not the usual dentistry . That is, for the resist.                  paul

-----Original Message-----
From: <Peter George Duncan> [mailto:[log in to unmask]]
Sent: Monday, May 28, 2001 3:39 PM
To: [log in to unmask]
Subject: [TN] Which Solder Mask


'Afternoon, All,

Today I need your help to find a good guide on how to select solder
mask/resist materials and how to determine what thickness should be
specified for particular applications. Immediately I need to know
recommendations for 0.063" thick, 10 layer FR4 HASL finished VME
conduction-cooled boards of 15 mil track spacing for military application.
Boards will be Convection Reflow Soldered with Kester 63/37 solder and 331
flux. Anything else you need to know?

I'm from a manufacturing background and have never needed to know this
level of detail before. However, I am now involved with helping a bunch of
design engineers who have even less idea than I do about this sort of thing
than I have. I have had a go at the Web trying various terms and key words,
but get absolutely nothing useful back at all, so I'm hoping our TechNet
Goldmine/Delphi Oracle can succeed where the WWW has failed me.

TIA,

Pete Duncan

----------------------------------------------------------------------------


-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------


-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2