TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Wolfe, Robert" <[log in to unmask]>
Date:
Tue, 8 Dec 1998 11:29:58 -0500
MIME-Version:
1.0
X-To:
David D Hillman <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Wolfe, Robert" <[log in to unmask]>
Parts/Attachments:
text/plain (117 lines)
Was this part of AMP's white paper material available on their WEB page or
was this in a book you can purchase.
Robert M. Wolfe

        -----Original Message-----
        From:   David D Hillman [SMTP:[log in to unmask]]
        Sent:   Monday, December 07, 1998 6:27 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] Gold and Tin Interconnect

        Hi Kenny - one more bit of information you may want to take a look
at -
        "Connector Contacts: Critical Surfaces", author Robert Mroczkowski
of AMP
        Inc, Advanced Materials & Processes inc. Metal Progress, 12/88,
pages
        49-52. This reference covers the basics very well and talks about
the
        pros/cons of tin. Good Luck.

        Dave Hillman
        Rockwell Collins
        [log in to unmask]





        Kenny Bloomquist <[log in to unmask]> on 12/02/98 10:29:34 AM

        Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please
respond
              to Kenny Bloomquist <[log in to unmask]>

        To:   [log in to unmask]
        cc:
        Subject:  [TN] Gold and Tin Interconnect




        We have an assembly that uses tin plated pins and sockets for the
        interconnection. We are having trouble getting the pin side in tin
but is
        readily available in gold. My question is "is there any long term
problems
        putting a gold pin in a tin plated socket"?

        For years people have put I/C leads into gold sockets without
problem so it
        seems that this should not be a problem but thought I'd ask for any
real
        life experiences.

        Thanks,

        Ken Bloomquist
        Sr. Principal Process Engineer
        PRIMEX Aerospace Company
        P.O. Box 97009
        Redmond, WA 98073-9709
        www.primextech.com

        Ph:   425-885-5000
        FAX: 425-882-5786
        [log in to unmask]

        Northcon/98, Show Director
        <www.northcon.org>

        Electronics Manufacturers Association (EMA), Secretary
        <www.ema-wa.org>

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following
        text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section
        for additional information.
        For technical support contact Hugo Scaramuzza at [log in to unmask] or
        847-509-9700 ext.312
        ################################################################

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
        For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
        ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2