Pete,
Seems to me there was recent thread here on something similar. We have soldered to stainless steel and I think the process is similar for aluminum. It has to do with the flux used. Word of caution... I believe it is an acid based flux so how it is applied and washed off may be of concern.
From McMaster-Carr website:
Aluminum Soldering Flux
Use this paste flux with aluminum solder and any tin/lead solder to solder aluminum and aluminum alloys. Also for use with copper, chrome, and brass. Meets DOD 1866 and is ROHS compliant.
4-oz. Jar 7696A2 Each $9.65
1-lb. Jar 7696A1 Each $30.41
I have not tried it.
Phil Nutting
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Houwen
Sent: Wednesday, October 29, 2008 10:01 AM
To: [log in to unmask]
Subject: [TN] Soldering to Aluminum?
Has anyone tried soldering lead free to an Aluminum circuit on polyester?
We are looking at a very simple one component circuit that needs to be on a
material with some flexibility. We do run millions of feet of aluminum on
polyester passive circuits in one of our plants. I am being asked to see if we
can take advantage of the in house production to save some cost.
My other thought is to just try a conductive adhesive, but we might need to
do some tooling for that, as this would require about 3 million of these
circuits/year.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|