Hello,

I have some questions regarding PCB for data and microwave applications
which I hope someone will give me some good inputs to.

Questions:

I would like to have some inputs abut solderability, shelf lifte etc. by
using different surface treatment onto the cu-pattern on a PCB. Your
experience by using:

a.	HAL
b.	Reflowed Sn/Pb
c.	Unreflowed Sn/Pb
d.	Electroless nickel/gold
e.           Organic passivation
f.	Other

And above surface treatments in combination with:

a.	Surface mounted chip components
b.	Surface mounted fine-pitch IC
c.	"Standard" hole mounted components 


Best Regards

Peter Dahlén

Saab Ericsson Space
[log in to unmask]
fax. +46 31 359520



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2