TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wS57W-000Bj1C; Thu, 15 May 97 13:19 CDT
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
<samples@[10.1.31.1]>
Date:
Thu, 15 May 1997 13:30:07 +0000
Precedence:
list
Comments:
Authenticated sender is <samples@[10.1.31.1]>
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
Priority:
normal
X-Status:
TO:
X-Loop:
Return-Path:
<TechNet-request>
>From bergdi Thu May 15 13:
19:49 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/12756
Resent-From:
Resent-Message-ID:
<"sAOa02.0.2JR.bErUp"@ipc>
From [log in to unmask] Mon May 19 09:
56:37 1997
Subject:
From:
"samples" <[log in to unmask]>
X-mailer:
Pegasus Mail for Windows (v2.52)
Reply-To:
Content-Transfer-Encoding:
7BIT
Message-Id:
Parts/Attachments:
text/plain (32 lines)
I am looking for some help on defining the differences 
between paste printing with stencil -vs- deposition (RPD) as it 
relates to how the paste performs in the oven. ie..slumping / oven 
profile differences.

The main issues I am tring to over come are:
1 Volume of paste ie..needle dia. / on time valve
2 Hot slumping conditions because the board has an extremely high 
   mass 250gms (multi-layer / heatsink plate)
3. The paste used is designed for deposition method

This assembly uses standard pitch (.050")  ceramic leadless chip 
carriers.  Can not screen print because of HS.


Thanks

Wesley Samples
Process Engineering Lead
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2