TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
[log in to unmask][log in to unmask] and I will compile the reply's and send them back to all
who reply.39_Pine.3.89.9506261015.C43764-0100000@ipc0_0_
Date:
Mon, 5 Jun 1995 11:01:42 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (16 lines)
Mr. Willis,
As far as I know, from my dealings as vice-chair of the Solder Mask Task
Group, no such reliable test method exists.  You might look for a method
which examines the change in capacitance with curing time.  I saw a
demonstration of it a few years ago, but never had the opportunity to pursue
the science.  The basic theory is that an uncured solder mask is applied over
a test pattern and the resistivity and capacitance are measured as the cure
cycle goes along.  When you have reached a point at which the two values are
only nominally changing, you have reached full cure.
I wish I could be of more help.  I guess memory is the first thing to go.

Doug Pauls aka [log in to unmask]