Fellow Techs,
We are assembling a double sided board with BGAs on both sides. One board
seems to be having a problem with a 21 mm sq. pbga that is initial installed
on the 1st side and then goes through the reflow oven again, upside down
during the 2nd side reflow. It looks like the bga is dropping slightly when
it goes through the reflow oven for a second time, upside down.
Does anyone have any ideas on how to either temporarily or permanently
secure the bga in place after the 1st side reflow so the bga does not pull
away from the board slightly during the 2nd side reflow? Tacking the
corners with some type of epoxy that would not affect long term reliability?
thanks
joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|