Fellow Techs, We are assembling a double sided board with BGAs on both sides. One board seems to be having a problem with a 21 mm sq. pbga that is initial installed on the 1st side and then goes through the reflow oven again, upside down during the 2nd side reflow. It looks like the bga is dropping slightly when it goes through the reflow oven for a second time, upside down. Does anyone have any ideas on how to either temporarily or permanently secure the bga in place after the 1st side reflow so the bga does not pull away from the board slightly during the 2nd side reflow? Tacking the corners with some type of epoxy that would not affect long term reliability? thanks joe --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------