TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Leonovich, Mike E." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 2 Aug 2000 14:40:40 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (44 lines)
Hi,

I've been trying to determine IPC specs for a particular Hot Air Solder
Leveling "defect".  Below is a electronic photo of the defect.



 <<...OLE_Obj...>>

This "defect" is called a solder tail, and I'm trying to determine when it's
actually a defect and why.

I know that if the "tail" stretches and contacts another annular ring, then
it's defective because of bridge or short.

If the surface plane of the annular ring is compromised by the excessive
solder at the base of the tail, then it's defective because the annular ring
needs to have a smooth even surface for the assembly of the surface mount.

Other than these issues, is there any other reason why this "tail" would be
defective?  If the presence of the tail doesn't create an uneven surface for
the annular ring, and if the tail doesn't contact any other features it
should be acceptable, right?

I appreciate whatever help you could give me.

Thanks.

Mike.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2