TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Date:
Fri, 23 Jan 2004 10:59:10 -0800
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Schleman, Joe A." <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (52 lines)
        Joe:
        It does not do anything to the boards nor components. Immersion
cleaning is used by mostly low volume outfits.
        In previous life we had an inline alcohol cleaner. It worked really
well. I have read many posts that say otherwise about alcohol but you can
not argue with facts.  What I saw was boards that came out clean and there
was no maintenance on the machine. We used it on boards that just came out
of the Wave Solder.
        Regards,
        Ramon

> -----Original Message-----
> From: Schleman, Joe A. [SMTP:[log in to unmask]]
> Sent: Friday, January 23, 2004 11:40 AM
> To:   [log in to unmask]
> Subject:      [TN] Soaking Circuit Boards in Alcohol
>
> Hi,
> I happened to observe somebody soaking some assembled boards in isopropyl
> alcohol to clean them. I was wondering if this was an acceptable method
for
> cleaning. I know using alcohol to clean is okay but, I'm not so sure about
> actually soaking the whole assembly in an alcohol bath. Any Insight would
be
> appreciated. Thanks.
>
> Joe
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2