Many years ago, I was involved in designing a computer by means of 20 layer
96 alumina boards 4x10 inches each, but it became so clumsy that we had to
change to LTCC. The boards had about 250 CCs. Today we use 96 alumina for
general purpose thickfilm circuits and 99 alumina for RF. What are you
asking for, manufacturing or CADing?
Inge
----- Original Message -----
From: "Harris Dy" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, May 07, 2009 9:21 PM
Subject: [TN] Material 96% Alumina
> Guys,
>
> Have any of you encountered "Material 96% Alumina" on PCB Fab Drawing? Any
> idea?
>
> Thanks,
> Harris
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|