Victor,
have a look at picture 10-49 and 10-50. There you can see SMD-Components
on lifted pads. But written criteria always take precedence over
illustrations.
There is no distinction between SMD and PTH Pads in the describing text.
Regards
Frank
Von: Victor Hernandez <[log in to unmask]>
An: <[log in to unmask]>
Datum: 07.08.2013 18:55
Betreff: [TN] IPC-610E, section 10.3.2, Conductors/Lands - Lifted
Pads/Lands (Con't)
Gesendet von: TechNet <[log in to unmask]>
Fellow TechNetters:
Can someone else interpret the stated criteria for section 10.3.2.
Figures 10-48 thru 50. Does this criteria solely pertain to
PTH/conductor lands or is this also pertain to Surface Mount Pads,
J-Leads, Gull Wing, SMT, etc.... I don't see how the industry can permit
lifted copper pads from the laminate. Is this criteria for Post
soldiering Process or what?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
.
Der Inhalt dieser E-Mail ist für den Absender rechtlich nicht verbindlich.
Informieren Sie uns bitte, wenn Sie diese E-Mail fälschlicherweise erhalten haben (Fax: +49-7551-891-4001). Bitte löschen Sie in diesem Fall die Nachricht. Jede Form der weiteren Benutzung ist untersagt.
.
The content of this e-mail is not legally binding upon the sender.
If this e-mail was transmitted to you by error, then please inform us accordingly (Fax: +49-7551-891-4001). In such case you are requested to erase the message. Any use of such e-mail message is strictly prohibited.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|