TECHNET Archives

June 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Rudy Sedlak <[log in to unmask]>
Date:
Tue, 24 Jun 2003 19:58:10 EDT
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (31 lines)
Effectively, a flux makes the oxides on the metal surface "go away", and
reveal bare metal, which the solder can bond to.

There really is two main ways to make oxides "go away", either reduce them to
metal, or dissolve them.

The rosin, and other, acids, which are in fluxes form salts with the metal in
the oxide, and either dissolve the salt in the flux fluid, or cause it to
ball up, and exit stage left as a sludge.

There are a whole raft of different ingredients in fluxes, and you choose
flux type, and thus ingredient type, depending on how aggressive you want your
flux, and what sort of residue you can tolerate on the surface after soldering.

This much is free...and remember, with free advice, it is often not worth
what you paid for it...

Rudy Sedlak
RD Chemical Company

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2