Effectively ALL fluxes are synthetic, except for pure water-white wood
rosin, which even may be, if you count distillation as a synthesis.
However, what you may be referring to is "Wally's Wonder Flux" which Dr
W. Rubin of Multicore developed in, I think, the early 1980s or late
1970s. I think the trade name was Xersin. This was like an activated
rosin flux except that the rosin was replaced by a synthetic polymer. It
was possibly the first true "no-clean" flux, because it required a
jackhammer to remove it :-)
Modern "no-clean" fluxes contain little or no resin/rosin and are mainly
a small quantity of dicarboxylic acids in a solvent/vehicle base.
Brian
Glenn Pelkey wrote:
> I must have been sleeping during the whole No-Clean introduction. I
> thought they were based on similar chemistries as Rosin, but with lower
> solids. A quick web search shows some are rosin, but most are
> "synthetic resin". The Resin definition says it is a derivative of
> Rosin. The MSDS of some say "Petroleum Distillates."
>
> So, can somebody explain what chemistry is in a No-Clean flux?
> What does "synthetic" actually mean?
>
> Thanks,
>
> Glenn
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|