What became of this question, Jong?
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: jong s kadesch [mailto:[log in to unmask]]
Sent: den 12 juni 2000 15:38
To: [log in to unmask]
Subject: [TN] GaAs Cracks
Hi Technetters,
Recently, I have attached GaAs die on a CVD diamond substrate using 80/20
Au/Sn eutectic preform. After the die bonding at 280 C, we found cracks
(mostly 90 degrees and 45 degrees cracks) on the surface of the GaAs during
the inspection. We suspect that it is due to TCE mismatch or thermal
shock. We are thinking about using different die attach material that
requires lower temperature process. Anyone has advise, suggestion, or any
experience similar to this? Thanks.
Jong S. Kadesch
Sr. Engineer
NASA-GSFC/Orbital Sciences Corp.
562/Component Technologies and Radiation Branch
Greenbelt, MD 20771
tel:(301)286-2785
fax:(301)286-1695
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|